跳至主要内容

Abrasion resistant ceramic lined pipe

Ceramic Lined Pipe, Ceramic Lined Elbows and Bends, Ceramic Tile Lined Pipes and Elbows , Bimetal Clad Pipe, Concrete Pump Pipe, Concrete Pump Boom Elbow, Honed Tubes for Hydraulic, Hard Chrome Plated Bars, Hydraulic Cylinder
SHS (Self-propagating High-temperature Synthetic process) ceramic lined steel pipe and elbow create a new generation of abrasion and corrosion resistant engineering pipeline.

The Manufacturing Process of Pipe and Elbow: 
SHS (Self-propagating High-temperature Synthetic process) ceramic lined steel pipe and elbow create a new generation of abrasion and corrosion resistant engineering pipeline.The composite steel pipe is composed of three layers: ceramic, intermediate, and steel layers. The ceramic layer is formed by molten alumina at a temperature above 2500 degree. The molten alumina produced from the reaction Fe2O3+2Al=2Fe+Al2O3 spreads on the inside wall of the steel pipe under the influence of a centrifugal force, then solidifies, so the ceramic layer has high density and smooth surface and bonds to the steel pipe.
Abrasion Resistant Ceramic Lined Pipes have been uniformly produced by a thermite reaction induced under the influence of a centrifugal force (Centrifugal Thermite Process) without any high-temperature furnace facilities. The characteristic feature of the present process for forming uniform ceramic layers is in its reaction propagation as well as the reaction heat and centrifugal force. It is very important in improving the quality of the ceramic lined pipes to find the proper conditions of the reactant and centrifugal force; the former mainly determines the produced ceramic layer quality and the latter the achievement of layer separation and the mechanical properties of the pipes.

Ceramic lined tube has great resistance against corrosion, abrasion and thermal shock. Features and Advantages:
1). High Abrasion Resistant: Vickers hardness of the corundum lining is HV1100 to1500, as high as that of tungsten-cobalt hard alloys, and the abrasion resistance is 20 times as carbon steel pipes. The composite ceramic lined steel elbow was used in a mining plant for about fifty thousands hours. The general service life of common steel elbow is about 700 hours.
2). Corrosion Resistant: Corundum is a neutral material, and is acid-proof and fouling -free.
3). Heat Resistant: Ceramic lined composite steel pipe can work under circumstances of -50 to 800 Celsius degree .
4). Lower Weight and Convenient Installation: The ceramic lined steel pipes are lighter than alloy pipes, cast iron pipes, and cast stone pipes and can be welded or connected through flanges, which reduces the expense of transportation and makes the pipes easier to install. For the pipes with the same sizes, types and length, the weight of ceramic pipe is about 1/2 of the wearable cast alloy steel pipe's, while the cost has reduced 10%~20% per meter. The weight of ceramic lined steel pipe is about 1/3 of the cast stone bent pipe's, 1/2 of the cast stone straight pipe's.
5). Lower Cost: Ceramic lined pipes can take place of expensive stainless steel, titanium, nickel, cast stone or alloy pipes. Extended service life can also reduce maintenance cost.

Specifications: 
Tube diameters:50 to 1020mm< Elbow angle: 22.5, 45, 60, 90, 120, 135, 150 degrees, etc. Three way pipes: Y shaped, Y lateral and other special shapes Four way pipes: straight cross, reducing cross. Ceramic lining thickness (including transition layer): 3 to 8mm

此博客中的热门博文

High Chromium Cast Iron Bimetal Cladding Pipe

High Chromium Cast Iron Bimetal Cladding Pipe, High Chromium Cast Iron pipe, Bimetal Cladding Pipe We are manufacturer of High Chromium Cast Iron Bimetal Cladding Pipe and supply high quality High Chromium Cast Iron Bimetal Cladding Pipe in both large and small quantities worldwide and offer you the best prices in the market. These Steel-high chromium cast iron bimetal cladding pipe is a new type of abrasion proof piping developed by our company. Outer of straight pipe is common steel pepe, cladding realized by forming high chromium lining via centrifugal forming technique. Outer of bend uses hot-bending bend and lining is cast with high-chromium cast iron. Compared with traditional wear-resistant alloy cast iron, wear-resistant alloy cast steel, general cladding steel pipe and cast stone pipe. 1. Good wear-resistance, giving full play to wear-resistance of high chromium cast iron. 2. Withstanding high pressure: It can be used for any pressure rating. Close bonding of outer and lining

ASME SA333 Gr.6 Seamless Steel Pipe

ASME SA333 Gr.6 Seamless Steel Pipe alloy steel ,  ASME SA333 Gr.6 ,  astm a333 ,  ASTM A333 Gr.6 ,  ASTM A333 Grade 6 ,  gr 6 ,  seamless steel pipe ASTM A333 Standard covers seamless and welded steel pipe for low temperature service. The Grade 6 steel involved is similar to AISI 4032 low alloy steel. ASTM A333 Grade 6 pipe shall be made by the seamless or welding process with the addition of no filler metal in the welding operation. Seamless and Welded Steel Pipe size for Low-Temperature Service: Outer Dimensions: 19.05mm-114.3mm Wall Thickness:2.0mm-14 mm Length: max 16000mm Application: Seamless and Welded Steel Pipe for Low-Temperature Service. Steel grade: ASTM A333 Grade 6 Inspection and Test: Chemical Composition Inspection, Mechanical Properties Test Tensile Strength,Yield Strength, Elongation, Flaring, Flattening, Bending, Hardness, Impact Test Surface and Dimension Test,No-destructive Test, Hydrostatic Test. ASTM A333 Gr. 6 Chemical Compositions(%) Elements Composition, % Ca

Silicon carbide alloy ceramic wear tube

Reaction bonded SiC is made by infiltrating compacts made of mixtures of SiC and carbon with liquid silicon. The silicon reacts with the carbon forming more SiC which bonds the initial SiC particles. Silicon carbide is formed in two ways, reaction bonding and sintering. Each forming method greatly affects the end microstructure. Reaction bonded SiC is made by infiltrating compacts made of mixtures of SiC and carbon with liquid silicon. The silicon reacts with the carbon forming more SiC which bonds the initial SiC particles. Sintered SiC is produced from pure SiC powder with non-oxide sintering aids. Conventional ceramic forming processes are used and the material is sintered in an inert atmosphere at temperatures up to 2000ºC or higher. Both forms of silicon carbide (SiC) are highly wear resistant with good mechanical properties, including high temperature strength and thermal shock resistance. Our engineers are always available to best advise you on the strengths and weaknesses of ea